doi: 10.1557/jmr.2012.351, Published by Cambridge University Press, 5 November 2012.
In Lu et al.1, the caption of Figs. 1(a) and 1(c) reads:
(a) 2-fold axis [1τ0] and (c) 5-fold axis [100].
It should read:
(a) 2-fold axis [100] and (c) 5-fold axis [1τ0]
The authors regret the error.
Reference
Lu Lu, Dongxia Xiong, Jianbo Wang, Dongshan Zhao, and Yufeng Sun: Varied Linear Phason Strain and Its Induced Domain Structure in Quasicrystalline Precipitates of Zr-Al-Ni-Cu-Nb Bulk Metallic Glass Matrix Composites. J. Mater. Res. 27(23), 3041–3048 (2012).
Rights and permissions
About this article
Cite this article
Lu, L., Xiong, D., Wang, J. et al. Varied linear phason strain and its induced domain structure in quasicrystalline precipitates of Zr-Al-Ni-Cu-Nb bulk metallic glass matrix composites–CORRIGENDUM. Journal of Materials Research 28, 658 (2013). https://doi.org/10.1557/jmr.2012.427