The construction of isothermal quaternary phase diagrams of the Na-M-O-S type for hot corrosion applications L. C. LiF. GesmundoF. Viani OriginalPaper Pages: 395 - 419
Initial oxidation of Cr at 300–730 K in H2 18O/H2 16O/16O2 gas mixtures studiedin situ with18O/SIMS and XPS Qin Lu OriginalPaper Pages: 421 - 432
High-temperature-sulfidation behavior of Fe-Mo-Mn-Al alloys Yisheng ChenD. J. YoungS. Blairs OriginalPaper Pages: 433 - 460
Thermal healing of mechanical defects on wüstite surfaces J. H. SwisherJ. Yang OriginalPaper Pages: 461 - 464
The spalling modes and degradation mechanism of ZrO2-8 wt.% Y2O3/CVD-Al2O3/Ni-22Cr-10Al-1Y thermal-barrier coatings J. H. SunE. ChangM. J. Cheng OriginalPaper Pages: 465 - 481
Evidence for the formation of substoichiometric species during internal oxidation of Ag-Mg alloys Luc CharrinAnnie CombeJean Cabane OriginalPaper Pages: 483 - 501
The growth and structure of thin oxide films on ceria-sol-coated nickel F. CzerwinskiW. W. Smeltzer OriginalPaper Pages: 503 - 527
Study of cracking and spalling of Cr2O3 scale formed on Ni-30Cr alloy Yifan ZhangDavid A. Shores OriginalPaper Pages: 529 - 553
Adherence behavior of oxide grown in air and synthetic exhaust gas on Fe-Cr-Al alloys containing strong sulfide-forming elements: Ca, Mg, Y, Ce, La, Ti, and Zr David R. Sigler OriginalPaper Pages: 555 - 583