Increasing the working life of machines I. KudryavtsevO. KulikovG. Zaitsev BriefCommunication Pages: 350 - 351
Thermomechanical treatment of pipes for the oil industry M. L. BernshteinN. Drégan Technology of Heat Treatment Pages: 352 - 356
Use of high frequency heating for heat treatment of drilling and casing pipes and turbodrill shafts and bodies N. V. ZiminV. G. Shevchenko Technology of Heat Treatment Pages: 357 - 360
Kinetics of the growth of austenite grains during isothermal induction heating K. Z. ShepelyakovskiiV. D. ZelenovaG. A. Ostrovskii Technology of Heat Treatment Pages: 361 - 364
Surface quenching after induction heating of cast iron cam shafts for ZIL-111 engines Yu. Ya. Postnikov Technology of Heat Treatment Pages: 365 - 366
Quenching in air-water mixtures D. V. BudrinV. M. Kondratov Technology of Heat Treatment Pages: 367 - 370
Effect of the tempering temperature on the properties of the products of decomposition of austenite within the intermediate and martensitic temperature ranges A. A. Sazonova Technology of Heat Treatment Pages: 371 - 373
Calculation of the time necessary to heat through and to cool steel machine parts during heat treatment N. I. Kobasko Technology of Heat Treatment Pages: 374 - 377
Heat treatment and mechanical properties of reinforcing steels L. E. Épshtein Technology of Heat Treatment Pages: 378 - 383
Structure and properties of welded high-strength titanium alloys L. A. GruzdevaA. I. Khorev Technology of Heat Treatment Pages: 384 - 385
Heat treatment of an alloy of the Ti−Al−Mo−Zr−Sn system E. K. MolchanovaV. A. Konstantinov Technology of Heat Treatment Pages: 386 - 387
Heat treatment of welded two-phase titanium alloys S. M. GurevichV. G. Grabin Technology of Heat Treatment Pages: 388 - 393
Heating semi-finished articles in molten glass L. B. EfimovaA. I. Kozlov Technical Information Pages: 394 - 395
Multinozzle gas burner for large and medium heat treatment furnace V. B. Modylevskii Technical Information Pages: 396 - 398
Effect of annealing on the creep resistance of tubular springs L. M. ButkevichM. P. Gridnev Technical Information Pages: 399 - 399
Analysis of ruptures of low alloyed steel with electron fractographs R. G. AroneP. I. SokolovskiiS. V. Bernshtein Technical Information Pages: 400 - 402
Heat treatment of case hardened hydroturbine parts P. I. Butkevich Technical Information Pages: 403 - 403
Cementite in the transition layer of steel-bronze bimetal V. S. PopovE. P. PonomarenkoL. G. Kravchenko Technical Information Pages: 404 - 406
Effect of heat treatment conditions on the ductility of Sv. 08GS steel M. G. PyatigorskiiE. T. Kondrat'ev Technical Information Pages: 410 - 410
New light high-modulus beryllium-aluminum alloys of the lockalloy type for space vehicles G. A. NekrasovaK. P. Yatsenko Technical Information Pages: 411 - 413