General features of the formation of the carburized layer in thermocyclic saturation S. F. Zabelin Chemicothermal Treatment Pages: 47 - 51
Carburizing titanium and cobalt alloys in propane with simultaneous formation of a carbon coating I. V. NikonorovaE. L. Gyulikhandanov Chemicothermal Treatment Pages: 52 - 53
Cyaniding steels with the use of triethanolamine L. P. Karpov Chemicothermal Treatment Pages: 54 - 58
Dependence of the recrystallization of austenite in boron steel 20G2R on the processes of temperature and strain treatment I. G. UzlovO. V. ParusovA. M. Nesterenko Technology of Heat Treatment Pages: 59 - 60
Stages of multiple fracture of low-alloy steels in a hydrogen sulfide medium L. R. BotvinaT. V. TetyuevaA. V. Ioffe Strength Pages: 61 - 70
An analysis of causes of embrittlement in chromium-nickel steels with titanium N. V. GoncharovaT. M. MakhnevaE. S. Makhnev Strength Pages: 71 - 75
Fundamental principles for choosing steels on the basis of results of wear tests G. M. SorokinS. N. Bobrov Friction. Wear Pages: 76 - 78
Structure and properties of steel after surface plastic deformation with simultaneous deposition of a coating A. N. Zavalishchin Friction. Wear Pages: 79 - 83
Depositing a wear-resistant coating on titanium alloys by oxidizing combined with aging N. S. Anan'inV. M. Polyanskii Friction. Wear Pages: 84 - 88