Abstract
We report scanning tunneling microscope observations of fracture surfaces formed during catastrophic crack growth in three metallic glasses: Ni56Cr18Si22B4, Co69Fe4Ni1Mo2B12Si12, and Fe78B13Si9. Macroscopically, the first two glasses fail along a slip band formed during loading and display a characteristic, μm-scale pattern of vein-like ridges; in contrast, Fe78B13Si9 displays little slip prior to fracture, and its fracture surface shows a μm-scale chevron pattern of steps. STM observations of fracture surfaces of all three materials show nm-scale grooves. The grooves in Co69Fe4Ni1Mo2B12Si12 are especially prominent and display stepped edges which we attribute to the intersection of shear bands with the surface. STM observations of the vein-like features on Ni56Cr18Si22B4 also show stepped edges. We attribute the vein features to the interaction of adjacent crack fingers in which the material between adjacent fingers fails in plane stress. The origin of the grooves is uncertain, but may be due to other shear instabilities along crack fingers.
Similar content being viewed by others
References
W. Klement, Jr., R.H. Willens, and P. Duwez, Nature 187, 869 (1960).
V. K. Sethi, R. Gibala, and A. H. Heuer, Scripta Metall. 12, 207 (1978).
CA. Pampillo, J. Mater. Sci. 10, 1194 (1975).
J. J. Oilman, J. Appl. Phys. 46, 1625 (1975).
R.W. Rice, in Fractography of Glasses and Ceramics, edited by J. R. Varner and V. D. Frechette (The American Ceramic Society, Westerville, OH, 1988), pp. 3–56.
L. A. Davis, in Metallic Glasses (American Society for Metals, Metals Park, OH, 1978), p. 190.
S.C. Langford, M. Zhenyi, L.C. Jensen, and J.T. Dickinson, J. Vac. Sci. Technol. A 8, 3470 (1990).
D. M. Kulawansa, S. C. Langford, and J. T. Dickinson, J. Mater. Res. 7, 1292 (1992).
K. Habib and A. Abdullah, J. Mater. Sci. Lett. 9, 1055 (1990).
R. Wiesendanger, M. Ringger, L. Rosenthaler, H. R. Hidber, P. Oelhafen, H. Rudin, and H-J. Güntherodt, Surf. Sci. 181, 46 (1987).
Y. Watanabe, J.T. Dickinson, D.M. Kulawansa, and S.C. Langford, Memoirs of the National Defense Academy, Japan 31, 53 (1992).
Y. Watanabe, T. Kubozoe, and Y. Nakamura, J. Mater. Res. 7, 1396 (1992).
Y. Watanabe and Y. Nakamura, J. Mater. Sci. Lett, (in press).
J.W. Lyding, S. Skala, J.S. Hubacek, R. Brockenbrough, and G. Gammie, Rev. Sci. Instrum. 59, 1897 (1988).
G. Reiss, J. Vancea, H. Wittmann, J. Zweck, and H. Hoffmann, J. Appl. Phys. 67, 1156 (1990).
G. Reiss, F. Schneider, J. Vancea, and H. Hoffmann, Appl. Phys. Lett. 57, 867 (1990).
C. A. Pampillo and H. S. Chen, Mater. Sci. Eng. 13, 181 (1974).
P. Diko, V. Ocelik, V. Hajko, Jr., J. Miskuf, and K. Csach, Kovove Materialy 25, 523 (1987).
R.E. Robertson and V.E. Mindroiu, Polym. Eng. Sci. 27, 55 (1987).
R.E. Robertson and V.E. Mindroiu, J. Mater. Sci. 20, 2801 (1985).
D.M. Kulawansa, J.T. Dickinson, S. C. Langford, and Y. Watanabe, unpublished.
N. I. Noskova, N. F. Vildanova, Yu. I. Filippov, and A. P. Potapov, Phys. Status Solidi A 87, 549 (1985).
E. Ben-Jacob, R. Godbey, N.D. Goldenfeld, J. Koplik, H. Levine, T. Mueller, and L.M. Sander, Phys. Rev. Lett. 55, 1315 (1985).
H. La Roche, J. F. Fernandez, M. Octavio, A. G. Loeser, and C. J. Lobb, Phys. Rev. A 44, R6185 (1991).
H.J. Leamy, H.S. Chen, and T.T. Wang, Metall. Trans. 3, 699 (1972).
F. Spaepen and D. Turnbull, Scripta Metall. 8, 563 (1974).
A.S. Argon and M. M. Salama, Mater. Sci. Eng. 23, 219 (1976).
H. U. Künzi, in Glassy Metals II: Atomic Structure and Dynamics, Electronic Structure, Magnetic Properties, edited by H. Beck and H-J. Güntherodt (Springer-Verlag, Berlin, 1983), pp. 169–216.
D. Broek, Elementary Engineering Fracture Mechanics, 4th ed. (Martinus Nijhoff, Dordrecht, The Netherlands, 1986), p. 113.
M.V. Swain, B.R. Lawn, and S.J. Burns, J. Mater. Sci. 9, 175 (1974).
Author information
Authors and Affiliations
Rights and permissions
About this article
Cite this article
Kulawansa, D.M., Dickinson, J.T., Langford, S.C. et al. Scanning tunneling microscope observations of metallic glass fracture surfaces. Journal of Materials Research 8, 2543–2553 (1993). https://doi.org/10.1557/JMR.1993.2543
Received:
Accepted:
Published:
Issue Date:
DOI: https://doi.org/10.1557/JMR.1993.2543