Corrosion and Anti-corrosion of Buried Pipeline

  • Chapter
  • First Online:
  • 889 Accesses

Abstract

The corrosion of buried pipeline is generated by its contact with soil. Soil corrosion is mainly related to the properties of the soil water. In this chapter, three corrosion reactions are introduced, including the corrosion generated when soil water contains oxygen, the corrosion generated when soil water contains acid gas, and the corrosion generated by bacteria in soil. Generally, anti-corrosion coating method and cathodic protection method are employed to reduce the corrosion of buried steel pipeline in the soil. Detained introduction to these two methods is given in this chapter.

This is a preview of subscription content, log in via an institution.

Buying options

Chapter
USD   29.95
Price excludes VAT (USA)
  • Available as PDF
  • Read on any device
  • Instant download
  • Own it forever
eBook
USD   129.00
Price excludes VAT (USA)
  • Available as EPUB and PDF
  • Read on any device
  • Instant download
  • Own it forever
Hardcover Book
USD   169.99
Price excludes VAT (USA)
  • Durable hardcover edition
  • Dispatched in 3 to 5 business days
  • Free shipping worldwide - see info

Tax calculation will be finalised at checkout

Purchases are for personal use only

Learn about institutional subscriptions

References

  • Bagnulo L (1985) Method of corrosion protection. US Patent 4,496,444, 29 Jan 1985

    Google Scholar 

  • Cao B (2006) Discussion on the selection of sacrificial anode sets in buried steel pipeline. Oil Gas Storage Transp 25(6):24–26, 30

    Google Scholar 

  • Chen S (1995) Paint process (updated version) first fascicle. Chemical Industry Press, Beijing, pp 1–20

    Google Scholar 

  • Feehan CE, Wagner EF (1977) Polyethylene coating for ferrous metals. US Patent 4,007,298, 8 Feb 1977

    Google Scholar 

  • Gay PJ (1975) Cathodic protection. US Patent 3,868,313, 25 Feb 1975

    Google Scholar 

  • Guo J, Wei C, Du X (2009) Development and new technology of pipeline coating. Pipeline Tech Equip 5:49–51

    Google Scholar 

  • Hielema R (1974) Pipe coating method. US Patent 3,823,045, 19 July 1974

    Google Scholar 

  • Hu S, Xu K, Wang W (1984) The make-in-research and application of Magnesium-base sacrifice anode. Oil Gas Storage Transp 3(4):37–41

    Google Scholar 

  • Huang H, Liu Y (2009) Cathodic protection technology and its application to buried steel pipeline. Pipeline Tech Equip (2):46–48, 51

    Google Scholar 

  • Jost JW, Ghandehari MH (1986) Corrosion protection with sacrificial anodes. US Patent 4,626,329, 2 Dec 1986

    Google Scholar 

  • Liu G (2007) Application of cathodic protection technology. Corros Prot Petrochem Ind 23(6):58–61

    Google Scholar 

  • Liu J, Wang W, Ma J (2006) Corrosion mechanisms of buried pipelines and countermeasures. Corros & Prot Petrochem Ind 23(6):20–22

    Google Scholar 

  • Liu P, Chen B, Guo D et al (2008) The origin and protect-ion research of the buried oil pipeline to corrode. Pipeline Tech Equip 4:47–48

    Google Scholar 

  • Moreland PJ, De Peuter FLJ (1995) Cathodic protection system and a coating and coating composition therefore. US Patent 5,431,795, 11 July 1995

    Google Scholar 

  • Ni Y (1994) Practical anti-corrosion techniques. Chemical Industry Press, Beijing, pp 195–209

    Google Scholar 

  • Norsworthy R (1998) Coating proves effective on hot pipelines. Pipeline Gas J 225(3):44–45, 48

    Google Scholar 

  • Oertel G (1985) Polyurethane handbook. Hanser Publishers, New York

    Google Scholar 

  • Torossian KA, Markovitz M, Cox FE (1986) Unique epoxy resin compositions and composite molded bodies filled therewith. US Patent 4,631,230, 23 Dec 1986

    Google Scholar 

  • Tran BT, Toerner TJ, Titus PE (1996) Polymer concrete coating for pipe, tubular shapes, other metal members and metal structures. US Patent 5,573,855, 12 Nov 1996

    Google Scholar 

  • Wang Y, Sun J (2007) External anticorrosive techniques on buried pipelines//China Petroleum and Natural Gas Co., Ltd. Xinjiang Oil Field Branch. Petroleum Industry Press, Beijing, pp 326–329

    Google Scholar 

  • Wang K, Wu J (1993) The development of soil corrosion mechanism and research technology. Prog Soil Sci 21(4):10–14

    Google Scholar 

  • Wang C, Pang Y, Li B (2009) Selection and installation of sacrificial anodes materials. Pipeline Tech Equip 1:59–60

    Google Scholar 

  • Wu J (1991) Effects of soil properties on electrode potential of steel in soils. Acta Pedologica Sinica 28(2):117–123

    Google Scholar 

  • Xiao J (1994) Corrosion introduction—corrosion of materials and control methods. Chemical Industry Press, Beijing, pp 284–296

    Google Scholar 

  • Yang Y (2005) Anti-corrosion progress of steel pipes. Petrochem Pipeline 28(3):39–40

    Google Scholar 

  • Yang J, Ma G, Zhang Y et al (2005) Selection and application on external coating of long-distance pipelines. Xinjiang Pet Sci & Technol 15(2):46–49

    Google Scholar 

  • Yu Z (1996) Paint process (updated version) second fascicle. Chemical Industry Press, Beijing, pp 496–497

    Google Scholar 

Download references

Author information

Authors and Affiliations

Authors

Corresponding author

Correspondence to Caili Dai .

Rights and permissions

Reprints and permissions

Copyright information

© 2018 Springer Nature Singapore Pte Ltd. and China University of Petroleum Press

About this chapter

Check for updates. Verify currency and authenticity via CrossMark

Cite this chapter

Dai, C., Zhao, F. (2018). Corrosion and Anti-corrosion of Buried Pipeline. In: Oilfield Chemistry. Springer, Singapore. https://doi.org/10.1007/978-981-13-2950-0_11

Download citation

Publish with us

Policies and ethics