Application of Suresh and Lee Models in the Measurement of Residual Stress of Coatings

Chapter
  • 683 Downloads

Abstract

Laser cladding is a green and potential surface hardening technology, which can be used to prepare high-quality coatings with high bonding strength, high hardness, and high toughness, thereby significantly improving wear resistance, corrosion resistance, and anti-fatigue performance of parts.

References

  1. 1.
    Chen J, Guo C, Zhou J. Microstructure and tribological properties of laser cladding Fe-based coating on pure Ti substrate. Trans Nonferrous Met Soc China. 2012;22:2171–8.CrossRefGoogle Scholar
  2. 2.
    Zhu LN, Xu BS, Wang HD, et al. Microstructure and nanoindentation measurement of residual stress in Fe-based coating by laser cladding. J Mater Sci. 2012;47(5):2122–6.CrossRefGoogle Scholar
  3. 3.
    Zheng BJ, Chen XM, Lian JS. Microstructure and wear property of laser cladding Al + SiC powders on AZ91D magnesium alloy. Opt Lasers Eng. 2010;48:526–32.CrossRefGoogle Scholar
  4. 4.
    Cui ZQ, Qin YC. Metallography and heat treatment (in Chinese). Beijing: China Machine Press; 2007.Google Scholar
  5. 5.
    Wang HD, Zhu LN, Xu BS. Measurement of residual stress of plasma sprayed Fe-based coating by nanoindentation (in Chinese). J Mech Eng. 2013;49(7):1–4.CrossRefGoogle Scholar
  6. 6.
    Zhu LN, Xu BS, Wang HD, et al. On the evaluation of residual stress and mechanical properties of FeCrBSi coatings by nanoindentation. Mater Sci Eng, A. 2012;536:98–102.CrossRefGoogle Scholar
  7. 7.
    Kuroda S, Clyne TW. The quenching stress in thermally sprayed coatings. Thin Solid Films. 1991;200:49–66.CrossRefGoogle Scholar
  8. 8.
    Zhao X, Xiao P. Residual stresses in thermal barrier coatings measured by photoluminescence piezospectroscopy and indentation technique. Surf Coat Technol. 2006;201:1124–31.CrossRefGoogle Scholar
  9. 9.
    Constable CP, Lewis DB, Yarwood J, et al. Raman microscopic studies of residual and applied stress in PVD hard ceramic coatings and correlation with X-ray diffraction (XRD) measurement. Surf Coat Technol. 2004;184:291–7.CrossRefGoogle Scholar
  10. 10.
    Zhang XC, Xu BS, Wang HD, et al. An analytical model for predicting thermal residual stresses in multilayer coating systems. Thin Solid Films. 2005;488:274–82.CrossRefGoogle Scholar
  11. 11.
    Xia D, Xu BS, Lv YH, et al. Influence of sweeping speed of deposition gun on Ni-based micro-plasma arc cladding coatings (in Chinese). Heat Treat Met. 2005;33(9):9–11.Google Scholar
  12. 12.
    Li HY. Indentation testing of residual stress and its mechanics for remanufacturing surface coatings (in Chinese). Master dissertation. Tianjin: Hebei University of Technology; 2011.Google Scholar
  13. 13.
    Jiang YP, Zhao GX, Pan Y. Mechanical properties of electrodeposited Ni coatings by nano indentation method (in Chinese). Nat Sci J Xiangtan Univ. 2005;27(3):50–8.Google Scholar
  14. 14.
    Wang HM, Xu BS, Ma SN. Preparation and micro mechanical properties of nano Al2O3 particles reinforced Ni-based composite coatings (in Chinese). Trans Mater Heat Treat. 2005;26(1):81–5.Google Scholar
  15. 15.
    Du LZ, Xu BS, Dong SY, et al. Preparation, microstructure and tribological properties of nano-Al2O3/Ni brush plated composite coatings. Surf Coat Technol. 2005;192:311–6.CrossRefGoogle Scholar
  16. 16.
    Wu Bin XuBS, Zhang B, et al. Preparation and properties of Ni/nano-Al2O3 composite coatings by automatic brush plating. Surf Coat Technol. 2007;201:6933–9.CrossRefGoogle Scholar
  17. 17.
    Gong JH, Wu JJ, Guan ZD. Analysis of the indentation size effect on the apparent hardness for ceramics. Mater Lett. 1999;38:197–201.CrossRefGoogle Scholar
  18. 18.
    Kim JY, Kang SK, Lee JJ, et al. Influence of surface-roughness on indentation size effect. Acta Mater. 2007;55:3555–62.CrossRefGoogle Scholar
  19. 19.
    Huang Y, Zhang F, Hwang KC, et al. A model of size effects in nano-indentation. J Mech Phys Solids. 2006;54:1668–86.CrossRefGoogle Scholar
  20. 20.
    Chang NK, Lin YS, Chen CY, et al. Size effect of indenter on determining modulus of nanowires using nanoindentation technique. Thin Solid Films. 2009;517:3695–7.CrossRefGoogle Scholar
  21. 21.
    Zhou YJ, Man HN. Generation of internal stress of plating layers and eliminating method (in Chinese). Coat Painting Electroplating. 2005;3(3):13–6.Google Scholar
  22. 22.
    Bouzakis KD, Skordaris G, Mirisidis J. Dermination of coating residual stress alterations demonstrated in the case of annealed films and based on a FEM supported continuous simulation of the nanoindentation. Surf Coat Technol. 2003;174:487–92.CrossRefGoogle Scholar
  23. 23.
    Hu GX, Cai X, Rong YH. Material science foundation (in Chinese). Shanghai: Shanghai Jiao Tong University Press; 2000.Google Scholar

Copyright information

© Springer Nature Singapore Pte Ltd. and Science Press 2018

Authors and Affiliations

  1. 1.National Key Laboratory for RemanufacturingAcademy of Armored Forces EngineeringBeijingChina
  2. 2.China University of GeosciencesBeijingChina

Personalised recommendations