Abstract
Crack initiation and propagation in saline ice were investigated in this study in an attempt to understand the processes of crack growth under low loading rates and variable temperatures. As has been previously observed in sea ice and freshwater ice, crack growth occurred in initiation/arrest increments. The energetic stability criterion of crack growth are examined and crack growth is characterized in terms of the fracture resistance-stress intensity factor K R . Salient features of this study are the development of a new fracture geometry capable of sustained crack growth over longer crack lengths and the presentation of a fracture resistance curve for saline ice.
Access this chapter
Tax calculation will be finalised at checkout
Purchases are for personal use only
Preview
Unable to display preview. Download preview PDF.
References
Dempsey, J.P., The fracture toughness of ice. In IUTAM/IAHR Symp. Ice/Struct., Springer-Verlag, 1989, (in press).
Dempsey, J.P., Wei, Y. and DeFranco, S.J., Fracture resistance to cracking in ice: initiation and growth, In Cold Regions Engineering, ed. D.S. Sodhi, ASCE, 1991, 579–594.
Parsons, B.L., Snellen, J.B. and Muggeridge, D.B., The initiation and arrest stress intensity factors of first year columnar sea ice. In 9th IAHR Ice Symp., 1988, 1, 502–512.
Parsons, B.L., Snellen, J.B. and Muggeridge, D.B., The double torsion test applied to fine grained freshwater columnar ice, and sea ice. In European Mechanics Colloquium 239, 1989, 188–200.
DeFranco, S.J. and Dempsey, J.P., Crack growth stability in S2 ice. 10th IAHR Ice Symp., 1990, 1, 168–181.
Williams, D. P. and Evans, A.G., A simple method for studying slow crack growth. J. Test. Eval., 1973, 1, 264–270.
Kanninen, M.F., An augmented double cantilever beam model for studying crack propagation and arrest. Int. J. Frac., 1973, 9, 83–92.
Ketcham, W.M. and Hobbs, P.V., An experimental determination of the surface energies of ice. Phil. Mag., 1969, 19, 1161–1173.
Gurney, C. and Hunt, J., Quasi-static crack propagation, Proc. Roy. Soc., 1967, A361, 254–263.
ASTM E561–86, 1987. R-curve determination. ASTM Stds, 03.01, 793–812.
Kanninen, M.F. and Popelar, C.H., Advanced Fracture Mechanics, Oxford University Press, New York, 1985, p. 212.
Mai, Y-W., Atkins, A.G., and Caddell, R.M., On the stability of cracking in wedge tapered DCB specimens. Int. J. Frac., 1975, 11, 939–953.
DeFranco, S.J., Wei, Y., and Dempsey, J.P., Notch acuity effects on the fracture toughness of saline ice. Annals of Glac., 1991, 15, in press.
Parsons, B.L., Subcritical crack growth, initiation and arrest in columnar freshwater and sea ice. Doctoral Thesis, Memorial University of Newfoundland, St. John’s, Newfoundland, 1989.
Author information
Authors and Affiliations
Editor information
Editors and Affiliations
Rights and permissions
Copyright information
© 1991 Elsevier Science Publishers Ltd
About this chapter
Cite this chapter
DeFranco, S.J., Dempsey, J.P. (1991). Crack Growth Stability in Saline Ice. In: Cocks, A.C.F., Ponter, A.R.S. (eds) Mechanics of Creep Brittle Materials 2. Springer, Dordrecht. https://doi.org/10.1007/978-94-011-3688-4_3
Download citation
DOI: https://doi.org/10.1007/978-94-011-3688-4_3
Publisher Name: Springer, Dordrecht
Print ISBN: 978-1-85166-701-7
Online ISBN: 978-94-011-3688-4
eBook Packages: Springer Book Archive