Built heritage consists to a large part of calcitic minerals (marble, limestone) which are prone to dissolution over a wide pH range. Indeed, chemical is solution is among the most significant factors contributing to the deterioration and damage of the built cultural heritage. Carbon dioxide dissolved in atmospheric water contributes to the development of acid conditions on the surface of the calcitic materials which accelerate dissolution of calcite crystals. These effects are enhanced in the case of polluted atmosphere which contributes to more aggressive environment for the dissolution process. The measurement of parameters that determine the kinetics of dissolution is very important for the understanding of dissolution mechanism and hence the design of efficient strategy for the prevention of it. As a result, precise and reproducible methods are necessary for drawing reliable mechanistic information. In the present work, the dissolution kinetics were investigated at conditions of constant driving force for the dissolution process. The methodology used to measure the rates of dissolution of calcitic marbles (>98% calcite) and sandstone was both accurate and highly reproducible. The rates of crystal dissolution measured were correlated with the corresponding solution undersaturation. The dissolution kinetics measurements showed that calcitic limestone at pH 8.25 had a lower dissolution rate constant in comparison with the respective value for Pentelic marble, a calcitic material (ca. 98% calcite). The mechanism was the same, i.e., surface diffusion controlled at alkaline pH values. The prevention of dissolution strategy therefore shall depend either on the alteration of fluid dynamics at the acid pH values or on the modification of the surfaces at the alkaline domain. The latter can be achieved by the addition of substances with functional groups, which may interact with the surface of the calcite crystals. Several inorganic ions (fluoride and sulfate) and one organic environmentally friendly compound, polycarboxymethyl inulin (CMI) (MW 15000), have been tested, and their effect on the rates of dissolution was discussed.

This is a preview of subscription content, log in via an institution to check access.

Access this chapter

Chapter
USD 29.95
Price excludes VAT (USA)
  • Available as PDF
  • Read on any device
  • Instant download
  • Own it forever
eBook
USD 169.00
Price excludes VAT (USA)
  • Available as EPUB and PDF
  • Read on any device
  • Instant download
  • Own it forever
Hardcover Book
USD 219.99
Price excludes VAT (USA)
  • Durable hardcover edition
  • Dispatched in 3 to 5 business days
  • Free shipping worldwide - see info

Tax calculation will be finalised at checkout

Purchases are for personal use only

Institutional subscriptions

References

  1. Baedecker PA, Reddy MM (1993) The Erosion of carbonate stone by acid rain. Laboratory and field investigations. J Chem Ed 70(2):104–108. https://doi.org/10.1021/ed070p104

    Article  CAS  Google Scholar 

  2. Graede TE (2000) Mechanisms for the atmospheric corrosion of carbonate stone. J Electrochem Soc 147(3):1006–1009. https://doi.org/10.1149/1.1393304. http://jes.ecsdl.org/content/147/3/1006.full.pdf+html

    Article  Google Scholar 

  3. Carrels RM, Christ CL (1966) Solutions, minerals and equilibrium. Harper and Row, New York, p 450

    Google Scholar 

  4. Krauskopf KB (1961) Introduction to geochemistry. McGraw-Hill, New York, p 721

    Google Scholar 

  5. Stumm W, Morgan J (1981) Aquatic chemistry, 2nd edn. Wiley, New York, p 780

    Google Scholar 

  6. Wang L, Nancollas GH (2008) Calcium orthophosphates: crystallization and dissolution. Chem Rev 108(11):4628–4669. https://doi.org/10.1021/cr0782574

    Article  CAS  Google Scholar 

  7. Kanellopoulou DG, Koutsoukos PG (2003) The calcite marble/water Interface: kinetics of dissolution and inhibition with potential implications in stone conservation. Langmuir 19(14):5691–5699. https://doi.org/10.1021/la034015x

    Article  CAS  Google Scholar 

  8. Xyla AG, Mikroyannidis J, Koutsoukos PG (1992) The inhibition of calcium carbonate precipitation in aqueous solutions by organophosphorus compounds. J Colloid Interface Sci 153(2):537–551. https://doi.org/10.1016/0021-9797(92)90344-L

    Article  CAS  Google Scholar 

  9. Knepper TP (2003) Synthetic chelating agents and compounds exhibiting complexing properties in the aquatic environment. Trends Anal Chem 22(10):708–724. https://doi.org/10.1016/S0165-9936(03)01008-2

    Article  CAS  Google Scholar 

  10. Guo J, Severtson SJ (2004) Inhibition of calcium carbonate nucleation with Aminophosphonates at high temperature, pH and ionic strength. Ind Eng Chem Res 43(17):5411–5417. https://doi.org/10.1021/ie049787i

    Article  CAS  Google Scholar 

  11. Spanos N, Kanellopoulou DG, Koutsoukos PG (2006) The interaction of diphosphonates with calcitic surfaces: understanding the inhibition activity in marble dissolution. Langmuir 22(5):2074–2081. https://doi.org/10.1021/la052062e

    Article  CAS  Google Scholar 

  12. Boels L, Witkamp GJ (2011) Carboxymethyl inulin biopolymers: a green alternative for phosphonate calcium carbonate growth inhibitors. Cryst Growth Des 11(9):4155–4165. https://doi.org/10.1021/cg2007183

    Article  CAS  Google Scholar 

  13. Demadis KD, Preari M (2013) Green scale inhibitors in water treatment processes: the case of silica scale inhibition. In: Proceedings of the 13th international conference on environmental science and technology, Athens, 5–7 Sept 2013, CEST2013_0280

    Google Scholar 

  14. Parkhurst DL, Appelo CAJ (2013) Description of input and examples for PHREEQC version 3 – a computer program for speciation, batch- reaction, one-dimensional transport, and inverse geochemical calculations: U.S. Geological Survey Techniques and Methods, Book 6, Chap. A43, 497 p. Available only at http://pubs.usgs.gov/tm/06/a43

  15. Cailleau P, Jaquin C, Dragone D, Girou A, Roques H, Humbert L (1979) Influence of foreign ions and of organic matter on the crystallization of calcium carbonates. Oil Gas Sci Technol Rev IFP 34(1):83–112. https://doi.org/10.2516/ogst:1979003. https://ogst.ifpenergiesnouvelles.fr/articles/ogst/abs/1979/01/vol34n1p83/vol34n1p83.html

    Article  CAS  Google Scholar 

  16. Tlili MM, Ben AM, Gabrielli C, Joiret S, Maurin G (2006) On the initial stages of calcium carbonate precipitation. Eur J Water Qual 37(1):89–108. https://www.scopus.com/inward/record.uri?eid=2-s2.0-33745142866&partnerID=40&md5=6905d0b52da80490b3dc22a88f7d0433

    CAS  Google Scholar 

  17. Paquette J, Vali H, Mucci A (1996) TEM study of Pt-C replicas of calcite overgrowths precipitated from electrolyte solutions. Geochim Cosmochim Acta 60(23):4689–4701. https://www.sciencedirect.com/science/journal/00167037/60/23

    Article  CAS  Google Scholar 

Download references

Acknowledgment

The authors wish to acknowledge support of the work from KRHPIS program – POLITEIA.

figure a

Author information

Authors and Affiliations

Authors

Corresponding author

Correspondence to Petros G. Koutsoukos .

Editor information

Editors and Affiliations

Rights and permissions

Reprints and permissions

Copyright information

© 2018 Springer International Publishing AG, part of Springer Nature

About this chapter

Check for updates. Verify currency and authenticity via CrossMark

Cite this chapter

Kanellopoulou, D.G., Koutsoukos, P.G. (2018). Kinetics of Dissolution of Monument Building Materials. In: Koui, M., Zezza, F., Kouis, D. (eds) 10th International Symposium on the Conservation of Monuments in the Mediterranean Basin. MONUBASIN 2017. Springer, Cham. https://doi.org/10.1007/978-3-319-78093-1_36

Download citation

Publish with us

Policies and ethics