Innovative Measurement Methodology in Quality Assessment of Coatings

  • Kenneth Moller
  • Anna Backman
  • Bo Carlsson
  • Magnus Palm
  • Sahar Al-Malaika
  • Husam Sheena
  • Elizabeth Lakin
  • Dieter Kockott
  • Bernd Dawid
  • Wolfgang Kortmann
  • Karl Bechtold
  • Jacques Simonin
  • Michael Hilt
  • Joachim Domnick
  • Dirk Michels
  • Axel Nagel
  • Manfred Wunsch
  • Karin Hvit Wernstal

Keywords

Coating System Hinder Amine Light Stabilizer Outdoor Exposure Accelerate Life Testing Service Life Prediction 
These keywords were added by machine and not by the authors. This process is experimental and the keywords may be updated as the learning algorithm improves.

Preview

Unable to display preview. Download preview PDF.

Unable to display preview. Download preview PDF.

References

  1. (1).
    Bauer, D.R. and Adamsons, K. (Chapter 9), Adamsons, K. (Chapter 10), and Gerlock, J.L., Smith, C.A., Cooper, V.A., Kaberline, S.A., Prater, T.J., Carter III, R.O., Kucherov, A.V., Misovski, T., and Nichols, M.E. (Chapter 11), in Service Life Prediction – Methodology and Metrologies, Martin, J.W. and Bauer, D.R. (Eds.), American Chemical Society Symposium Series 805, Oxford University Press, Washington, DC, 2001.Google Scholar
  2. (2).
    Bauer, D.R. and Dickie, R.A., “Crosslinking Chemistry and Network Structure in Organic Coatings. I. Cure of Melamine Formaldehyde/Acrylic Copolymer Films,” J. Polym. Sci., Polym. Phys., 18 1997-2014 (1980).CrossRefGoogle Scholar
  3. (3).
    Adamsons, K., “Chemical Surface Characterization and Depth Profiling of Automotive Coating Systems,” Prog. Polym. Sci., 25 (9) 1363-1409 (2000).CrossRefGoogle Scholar
  4. (4).
    Haacke, G., Brinen, J.S., and Larkin, P.J., “Depth Profiling of Acrylic/Melamine Formaldehyde Coatings.“ J. Coat. Technol., 67, >No. 843, 29-34 (1995).Google Scholar
  5. (5).
    Adamsons, K., Short Course Presentation at the Atlas School or Natural and Accelerated Weathering (ASNAW), April 28-30, Miami, FL, 1999.Google Scholar
  6. (6).
    Gerlock, J.L., Smith, C.A., Cooper, V.A., Dusbiber, T.G., Weber, W.H., “On the Use of Fourier Transform Infrared Spectroscopy and Ultraviolet Spectroscopy to Assess the Weathering Performance of Isolated Clearcoats from Different Chemical Families,” Polym. Degrad. Stab., 62, 225-234 (1998).CrossRefGoogle Scholar
  7. (7).
    Adamsons K., Sticka, K., Swartzfager, D., Walls, D., Wood, B., and Lloyd, K., “Characterization of Multilayered Automotive Paint Systems Including Depth Profiling and Interface Analysis,” Polym. Mater. Sci. Eng., 77 482-483 (1996).Google Scholar
  8. (8).
    Gerlock, J., Prater, T., Kaberline, S., and deVries, J.E., “Assessment of Photooxidation in Multi-Layer Coating Systems by Time-Of-Flight Secondary Ion Mass Spectrometry,” J. Polymer Deg. Stab., 47, 405-411 (1995).CrossRefGoogle Scholar
  9. (9).
    Moller, K., Jansson, A., and Sjovall, P., “Analysis of Polymer Oxidation Using 18O2 and TOFSIMS,” J. Polymer Deg. Stab., 80, 345-353, 2003.CrossRefGoogle Scholar
  10. (10).
    Moller, K., Backman, A., and Johansson, U., “Analysis of Photooxidation of Automotive Coating Systems Using 18O2 and TOF-SIMS,” Third MoDeSt Conference in Lyon, August-September, 2004.Google Scholar
  11. (11).
    Bauer, D.R., “Chemical Criteria for Durable Automotive Topcoats,” J. Coat. Technol., 66, No. 835, 57-65 (1994).Google Scholar
  12. (12).
    Haacke, G., Andrawes, F.F., Cambell, B.H., “Migration of Light Stabilizers in Acryl/Melamine Clearcoats,” J. Coat. Technol., 68, No. 855, 57-62 (1996).Google Scholar
  13. (13).
    Haacke, G., Longordo, E., Brinen, J.S., Andrawes, F.F., Cambell, B.H., “Chemisorption and Physical Adsorption of Light Stabilizers in Pigments and Ultrafine Particles,” J. Coat. Technol., 71, No. 888, 87-94 (1999).CrossRefGoogle Scholar
  14. (14).
    Haacke, G., Longordo, E., Brinen, J.S., Andrawes, F.F., Cambell, B.H., Proc. 25th Int. Waterborne, High-Solids, Powder Coat. Symp., 433-443, 1998.Google Scholar
  15. (15).
    Haacke, G., Longordo, Andrawes, F.F., and Cambell, B.H., “Interaction Between Light Stabilizers and Pigment Particles in Polymeric Coatings,” Prog. Org. Coat., 34, 75-83 (1998).CrossRefGoogle Scholar
  16. (16).
    Adamsons, K., Short Course Presentation at the Atlas School of Natural and Accelerated Weathering (ASNAW), April 28-30, Miami, FL, 1999.Google Scholar
  17. (17).
    Moller, K. and Gevert, T., “A Solid State Analysis of the Desorption/Evaporation of Hindered Phenols from Low Density Polyethylene (LDPE) Using FTIR and UV Spectroscopy Integrating Sphere: The Effect of Molecular Size on the Desorption,” J. Appl. Polym. Sci., 61, 1149-1162 (1996).CrossRefGoogle Scholar
  18. (18).
    Jorgensen, G., Brunold, S., Carlsson, B., Heck, M., and Moller, K., Performance and Durability Assessment: Optical Materials for Solar Thermal Systems, Koehl, M., Carlsson, B., Jorgensen, G.J., and Czanderna, A.W. (Eds.), Chapter 6, Elsevier, Oxford, 2004.Google Scholar

Copyright information

© Springer Science+Business Media, LLC 2009

Authors and Affiliations

  • Kenneth Moller
    • 1
  • Anna Backman
    • 1
  • Bo Carlsson
    • 1
  • Magnus Palm
    • 1
  • Sahar Al-Malaika
    • 2
  • Husam Sheena
    • 2
  • Elizabeth Lakin
    • 2
  • Dieter Kockott
    • 3
  • Bernd Dawid
    • 4
  • Wolfgang Kortmann
    • 4
  • Karl Bechtold
    • 5
  • Jacques Simonin
    • 5
  • Michael Hilt
    • 6
  • Joachim Domnick
    • 7
  • Dirk Michels
    • 7
  • Axel Nagel
    • 8
  • Manfred Wunsch
    • 8
  • Karin Hvit Wernstal
    • 9
  1. 1.SP Technical Research Institute of SwedenBorasSweden
  2. 2.Aston UniversityBirminghamUK
  3. 3.Atlas MTT BVLochemThe Netherlands
  4. 4.BYK-ChemieWeselGermany
  5. 5.ClariantHuningueFrance
  6. 6.DaimlerChryslerSindelfingenGermany
  7. 7.FhG-IPAStuttgartGermany
  8. 8.PPGIngersheimGermany
  9. 9.Volvo Car CorporationGothenburgSweden

Personalised recommendations