Advertisement

Ductile Mode Cutting Characteristics

  • Kiu LiuEmail author
  • Hao Wang
  • Xinquan Zhang
Chapter
Part of the Springer Series in Advanced Manufacturing book series (SSAM)

Abstract

Ductile mode cutting characteristics and material removal mechanism of brittle material are discussed using tungsten carbide as an example work material in this chapter. Grooving and milling tests are designed and conducted to investigate their cutting modes. Experimental results indicate that there is a transition from ductile mode cutting to brittle mode cutting in grooving of tungsten carbide when depth of cut is increased from zero to a certain value. SEM observations on machined work surfaces show that there are three cutting modes in grooving of brittle material as depth of cut being increased: ductile mode cutting, semi-brittle mode cutting and brittle mode cutting. Cutting modes is identified and classified by machined surface texture and chip formation. In ductile mode cutting of tungsten carbide, thrust force Ft is much larger than cutting force Fc, which results in a large compressive stress in cutting zone. Large compressive stress and shear stress could shield the growth of pre-existing flaws in work material by suppressing its stress intensity factor KI, such that KI < KC making work material is able to undertake a large cutting stress without fracturing to achieve ductile mode cutting. SEM and EDS examinations on cutting tools indicate that tool wear mainly occurs on flank face and tool wear mechanisms are dominated by diffusion, adhesion and abrasion in cutting of tungsten carbide.

References

  1. 1.
    Liu K (2002) Ductile cutting for rapid prototyping of tungsten carbide tools. NUS Ph.D. thesis, SingaporeGoogle Scholar
  2. 2.
    Liu K, Li XP (2001) Modelling of ductile cutting of tungsten carbide. Trans NAMRI/SME 29:251–258Google Scholar
  3. 3.
    Liu K, Li XP (2001) Ductile cutting of tungsten carbide. J Mater Process Technol 113:348–354CrossRefGoogle Scholar
  4. 4.
    Liu K, Li XP, Rahman M et al (2004) A study of the cutting modes in grooving of tungsten carbide. Int J Adv Manuf Technol 24:321–326CrossRefGoogle Scholar
  5. 5.
    Liu K, Li XP, Liang SY (2004) Nanometer scale ductile cutting of tungsten carbide. J Manuf Process 6:187–195CrossRefGoogle Scholar
  6. 6.
    Liu K, Li XP, Rahman M et al (2003) CBN tool wear in ductile cutting of tungsten carbide. Wear 255:1344–1351CrossRefGoogle Scholar
  7. 7.
    Liu K, Li XP, Liang SY (2007) The mechanism of ductile chip formation in cutting of brittle materials. Int J Adv Manuf Technol 33:875–884CrossRefGoogle Scholar
  8. 8.
    Li XP, Rahman M, Liu K et al (2003) Nano-precision measurement of diamond tool edge radius for wafer fabrication. J Mater Process Technol 140:358–362CrossRefGoogle Scholar
  9. 9.
    Upadhyaya GS (1996) Nature and properties of refractory carbides. Nova Science Publishers, New York, pp 213–292Google Scholar
  10. 10.
    Pierson HO (1996) Handbook of refractory carbides and nitrides: properties, characteristics, processing and applications. Noyes Publications, New Jersey, pp 100–116CrossRefGoogle Scholar
  11. 11.
    Topper TH, Yu MT (1985) The effect of overloads on threshold and crack closure. Int J Fatigue 7:159–164CrossRefGoogle Scholar
  12. 12.
    Barry J, Byrne G (2001) Cutting tool wear in the machining of hardened steels, part II: cubic boron nitride cutting tool wear. Wear 247:152–160CrossRefGoogle Scholar
  13. 13.
    Liu K, Li XP, Liang SY et al (2005) Nanometer scale ductile mode cutting of soda-lime glass. J Manuf Process 7:95–101CrossRefGoogle Scholar
  14. 14.
    Moriwaki T, Shmoto E, Inoue K (1992) Ultraprecision ductile cutting of glass by applying ultrasonic vibration. CIRP Ann 41:141–144CrossRefGoogle Scholar
  15. 15.
    Antwi EK, Liu K, Wang H (2018) A review on ductile mode cutting of brittle materials. Front Mech Eng 13:251–263CrossRefGoogle Scholar
  16. 16.
    Liu K, Li XP, Liang SY et al (2004) Nanometer scale ductile mode cutting of soda-lime glass. Trans NAMRI SME 32:39–45Google Scholar
  17. 17.
    Fang FZ, Chen LJ (2000) Ultra-precision cutting for ZKN7 glass. CIRP Ann 49:17–20CrossRefGoogle Scholar
  18. 18.
    Zhou M, Wang XJ, Ngoi BK et al (2002) Brittle ductile transition in the diamond cutting of glasses with the aid of ultrasonic vibration. J Mater Process Technol 121:243–251CrossRefGoogle Scholar
  19. 19.
    Fang FZ, Venkatesh VC (1998) Diamond cutting of silicon with nanometric finish. CIRP Ann 47:45–49CrossRefGoogle Scholar
  20. 20.
    Zhang JG, Zhang JJ, Cui T et al (2017) Sculpturing of single crystal silicon microstructures by elliptical vibration cutting. J Manuf Process 29:389–398CrossRefGoogle Scholar
  21. 21.
    Liu K, Li XP, Rahman M (2003) Characteristics of high speed micro cutting of tungsten carbide. J Mater Process Technol 140:352–357CrossRefGoogle Scholar

Copyright information

© Springer Nature Singapore Pte Ltd. 2020

Authors and Affiliations

  1. 1.Singapore Institute of Manufacturing TechnologySingaporeSingapore
  2. 2.Department of Mechanical EngineeringNational University of SingaporeSingaporeSingapore
  3. 3.School of Mechanical EngineeringShanghai Jiao Tong UniversityShanghaiChina

Personalised recommendations