Abstract

High-concentration Al–Ti–B master alloy was prepared by melt self-propagating high-temperature synthesis, and then the extruder bar of intermediate alloy was also prepared. The grain refiner can be divided into two categories. One is TiB2 particles only, and the other is two particulate matter containing both TiB2 and TiAl3. The microstructures of the two-grain refiners were observed under scanning electron microscope (SEM) and compared with the commercial refiners. The fining effects of the two-grain refiners were analyzed. The refining mechanism of TiAl3 and TiB2 was discussed, and the optimum dosage and the refinement scheme of pure aluminum were optimized.

Keywords

Aluminum alloy Grain refiner Microstructure Refinement effect 

References

  1. 1.
    H.B. Michael Rajan, S. Ramabalan, I. Dinaharan, S.J. Vijay, Synthesis and characterization of in situ formed titanium diboride particulate reinforced AA7075 aluminum alloy cast composites. Mater. Des. 44, 438–445 (2013)CrossRefGoogle Scholar
  2. 2.
    Y. Ma, Z. Chen, M. Wang, D. Chen, N. Ma, H. Wang, High cycle fatigue behavior of the in-situ TiB2/7050 composite. Mater. Sci. Eng., A 640, 350–356 (2015)CrossRefGoogle Scholar
  3. 3.
    C. Dong, L. Yongkang, B. Liang, M. Naiheng, L. Xian-feng, W. Haowei, Mechanical properties and microstructure of in situ TiB27055 composites. Chin. J. Aeronaut. 19, S66–S70 (2006)Google Scholar
  4. 4.
    Zhong L-h, Zhao Y-t, Zhang S-l, G. Chen, S. Chen, Liu Y-h, Microstructure and mechanical properties of in situ TiB2/7055 composites synthesized by direct magnetochemistry melt reaction. Trans. Nonferrous Metals Soc. China 23(9), 2502–2508 (2013)CrossRefGoogle Scholar
  5. 5.
    D. Chen, C. Zou, Y.J. Zhang, N.H. Ma, H.W. Wang, Tensile properties of 15wt. %TiB2/7055 composite fabricated by in situ method. Adv. Mater. Res. 842, 165–169 (2013)CrossRefGoogle Scholar
  6. 6.
    C. Yuanshenru, S. Jienlin, Ageing behaviour of SiCp-reinforced AA 7075 composites. J. Mater. Sci. 32, 1741–1747 (1997)CrossRefGoogle Scholar
  7. 7.
    N.V.R. Kumar, E.S. Dwarakadasa, Effect of matrix strength on the mechanical properties of Al–Zn–Mg/SiC P, composites. Compos. A Appl. Sci. Manuf. 31(10), 1139–1145 (2000)CrossRefGoogle Scholar
  8. 8.
    N.V.R. Kumar, E.S. Dwarakadasa, Effect of matrix strength on the mechanical properties of Al–Zn–Mg/SiCP composites. Compos. A Appl. Sci. Manuf. 31, 1139–1145 (2000)CrossRefGoogle Scholar
  9. 9.
    W. Yuan, J. Zhang, C. Zhang, Z. Chen, Processing of ultra-high strength SiCp/Al–Zn–Mg–Cu composites. J. Mater. Process. Technol. 209, 3251–3255 (2009)CrossRefGoogle Scholar
  10. 10.
    Das DK, Mishra PC, Chaubey AK, Singh S. Fabrication process optimization for improved mechanical properties of Al 7075/SiCp metal matrix composites. Manag. Sci. Lett., 297–308 (2016)Google Scholar

Copyright information

© Springer Nature Singapore Pte Ltd. 2019

Authors and Affiliations

  • Mengke He
    • 1
  • Lihua Chai
    • 1
  • Hongda Wang
    • 1
  • Ziyong Chen
    • 1
    Email author
  • Yapeng Cui
    • 1
  1. 1.College of Materials Science and EngineeringBeijing University of TechnologyBeijingChina

Personalised recommendations