Abstract
The purpose of the present research work is to study the structural, mechanical and wear properties of artificial hip ceramic composites with varying proportion of aluminum and chromium oxide. The ceramic composites containing fixed amount of zirconium oxide, magnesium oxide, silicon nitride with varying amount of aluminum and chromium oxide were fabricated by using spark plasma sintering process and subsequently evaluated for structural (XRD, X-ray diffraction), elemental (EDS, energy-dispersive spectroscopy), mechanical (fracture toughness, elastic modulus and hardness) and wear properties. The results showed that aluminum and chromium oxide contents have a significant influence on the mechanical and wear properties of the fabricated ceramic composites. In particular, the composites containing 1.5 wt% chromium oxide and 70.5 wt% of aluminum oxide showed better mechanical properties with improved wear resistance. This result clearly indicates that the proposed ceramic materials may be a better alternative for artificial hip material.
Keywords
This is a preview of subscription content, log in via an institution.
Buying options
Tax calculation will be finalised at checkout
Purchases are for personal use only
Learn about institutional subscriptionsReferences
Trindade, M.C.D., Lind, M., Sun, D., Schurman, D.J., Goodman, S.B., Smith, R.L.: In vitro reaction to orthopaedic biomaterials by macrophages and lymphocytes isolated from patients undergoing revision surgery. Biomaterials 22(3), 253–259 (2001)
Hu, D., Tie, K., Yang, X., Tan, Y., Alaidaros, M., Chen, L.: Comparison of ceramic-on-ceramic to metal-on-polyethylene bearing surfaces in total hip arthroplasty: a meta-analysis of randomized controlled trials. J. Orthop. Surg. Res. 10, 22 (2015). https://doi.org/10.1186/s13018-015-0163-2
Mattei, L., Di Puccio, F., Piccigallo, B., Ciulli, E.: Lubrication and wear modelling of artificial hip joints: a review. Tribol. Int. 44, 532–549 (2011)
Skinner J.A., Haddad F.S.: Ceramics in total hip arthroplasty: a bearing solution?. Bone Joint J. 99-B(8), 993–995 (2017)
Yoshitoshi, H., Yukiharu, H., Taisuke, S., Daigo, K., Naoki, I.: Significantly lower wear of ceramic-on-ceramic bearings than metal-on-highly cross-linked polyethylene bearings: A 10- to 14-year follow-up study. J. Arthroplast. 31(6), 1246–1250 (2016)
Vendittoli, P.A., Amzica, T., Roy, A.G., Lusignan, D., Girard, J., Lavigne, M.: Metal ion release with large-diameter metal-on-metal hip arthroplasty. J. Arthroplast. 26(2), 282–288 (2011)
Smeekes, C., Ongkiehong, B., Van der Wal, B., Wolterbeek, R., Henseler, J.F., Nelissen, R.: Large fixed-size metal-on-metal total hip arthroplasty: higher serum metal ion levels in patients with pain. Int. Orthop. 39(4), 631–638 (2015)
Bizot, P., Nizard, R., Lerouge, S., Prudhommeaux, F., Sedel, L.: Ceramic/ceramic total hip arthroplasty. J. Orthop. Sci. 5, 622–627 (2000)
Rahman, H.S.A., Choudhury, D., Osman, N.A.A., Shasmin, H.N., Abas, W.A.B.W.: In vivo and in vitro outcomes of alumina, zirconia and their composited ceramic-on-ceramic hip joints. J. Ceram. Soc. Jpn. 121(4), 382–387 (2013)
Bahraminasab, M., Sahari, B.B., Edwards, K.L., Farahmand, F., Arumugam, M., Hong, T.S.: Aseptic loosening of femoral components—a review of current and future trends in materials used. Mater. Des. 42, 459–470 (2012)
Silva, C.C.G.E., Higa, O.Z., Bressiani, J.C.: Cytotoxic evaluation of silicon nitride-based ceramics. Mater. Sci. Eng., C 24, 643–646 (2004)
Bal, B.S., Khandkar, A., Lakshminarayanan, R., Clarke, I., Hoffman, A.A., Rahaman, M.N.: Fabrication and testing of silicon nitride bearings in total hip arthroplasty. J. Arthroplast. 24(1) (2009)
Nevelos, J.E., Prudhommeaux, F., Doyle, M., Hamadouche, C., Ingham, E., Meunier, A., Nevelos, A.B., Sedel, L., Fisher, J.: Comparative analysis of two different types of alumina-alumina hip prosthesis retrieved for aseptic loosening. J. Bone Joint Surg. (Br) 83-B, 598–603 (2011)
Jenabzadeh, A.R., Pearce, S.J., Walter, W.L.: Total hip replacement: ceramic-on-ceramic. Semin. Arthroplast. 23(4), 232–240 (2012)
Anstis, G.R., Chantikul, P., Lawn, B.R., Marshall, D.B.: A critical evaluation of indentation techniques for measuring fracture toughness: I. Direct crack measurements. J. Am. Ceram. Soc. 64(9), 533–538 (1981)
International Standards, ISO-6474-2-2012 (en): Implants for surgery Ceramic materials -Part 2: Composite materials based on a high-purity alumina matrix with zirconia reinforcement. 04 (2012)
International Standards, ISO-23317: Implants for Surgery-In Vitro Evaluation for Apatite-Forming Ability of Implant Materials, 1st edn (2007)
Author information
Authors and Affiliations
Corresponding author
Editor information
Editors and Affiliations
Rights and permissions
Copyright information
© 2019 Springer Nature Singapore Pte Ltd.
About this paper
Cite this paper
Goswami, C., Patnaik, A., Bhat, I.K., Singh, T. (2019). Synthesis and Characterization of Al2O3–Cr2O3-Based Ceramic Composites for Artificial Hip Joint. In: Chandrasekhar, U., Yang, LJ., Gowthaman, S. (eds) Innovative Design, Analysis and Development Practices in Aerospace and Automotive Engineering (I-DAD 2018). Lecture Notes in Mechanical Engineering. Springer, Singapore. https://doi.org/10.1007/978-981-13-2718-6_3
Download citation
DOI: https://doi.org/10.1007/978-981-13-2718-6_3
Published:
Publisher Name: Springer, Singapore
Print ISBN: 978-981-13-2717-9
Online ISBN: 978-981-13-2718-6
eBook Packages: EngineeringEngineering (R0)