Abstract
With the investigated subject of 82B rod, the interlamellar spacings of pearlite at different isothermal transformation temperatures and different cooling rates during continuous cooling transformation were measured, and the effect of the isothermal transformation temperature and cooling rate on the interlamellar spacing was analyzed quantitatively. Moreover, the relationship models between undercooling and interlamellar spacing were presented by data regression. The experimental results show that the relationship between undercooling and reciprocal interlamellar spacing remains linear when the undercooling is not very large, or else, the interlamellar spacing tends to be constant and the relationship will deviate from linearity.
Similar content being viewed by others
References
WANG You-ming, LI Man-yun, WEI Guang. Controlled Rolling and Controlled Cooling of Steels [M]. Beijing: Metallurgical Industry Press, 2005 (in Chinese).
XU Zu-yao. Theory of Phase Transformation [M]. Beijing: The Science Press, 1998 (in Chinese).
Puls M P, Kirkaldy J S. The Pearlite Reaction [J]. Metallurgical Transactions, 1972, (3): 2777.
Hillert M, Hoglund L. Comments on Kinetics Model of Isothermal Pearlite Formation in a 0.4C-1. 6Mn Steel [J]. Scripta Materialia, 2004, 50(1): 171.
Satio Y. Modelling of Microstructural Evolution in Thermome-chanical Processing of Structural Steels [J]. Materials Science and Engineering, 1997, 223A: 134.
Phadke S, Pauskar P, Shivpuri R. Computational Modeling of Phase Transformations and Mechanical Properties During the Cooling of Hot Rolled Rod [J]. Journal of Materials Processing Technology, 2004, 150: 107.
Kazeminezhad M, Taheri A K. The Effect of Controlled Cooling After Hot Rolling on the Mechanical Properties of a Commercial High Carbon Steel Wire Rod [J]. Materials and Design, 2003, 24: 415.
Author information
Authors and Affiliations
Corresponding author
Rights and permissions
About this article
Cite this article
Xu, Jq., Liu, Yz. & Zhou, Sm. Calculation models of interlamellar spacing of pearlite in high-speed 82B rod. J. Iron Steel Res. Int. 15, 57–60 (2008). https://doi.org/10.1016/S1006-706X(08)60144-2
Revised:
Published:
Issue Date:
DOI: https://doi.org/10.1016/S1006-706X(08)60144-2