Abstract
Transverse to pipe axis cracks across the weld line of high frequency-electrical resistance weld (HF-ERW) pipes of IS 10748 Grade 2 and size 406.4 mm outside diameter and 7.75 mm wall thickness were observed. Analytical techniques such as ultrasonic testing, optical microscopy and scanning electron microscopy with energy-dispersive spectroscopy were used for analysis and determination of the root cause.
Similar content being viewed by others
References
D. Li, Y. Peng, J. Mater. Process. Technol. 209, 4850–4856 (2009)
A. Kainz, S. Ilie, E. Parteder, K. Zeman, Steel Res. Int. 79(11), 861–867 (2008)
T. Kyada, J. Raghu Shant, R.K. Goyal, T.S. Kathayat, J. Fail, Anal. Prev. 15(2), ISSN 1547-7029 (2015)
E. Ervasti, U. Stahlberg, J. Mater. Process. Technol. 101(1), 312–321 (2000)
Acknowledgments
The authors are grateful to HFW Pipe Plant and MSU Baroda for supporting part of this analysis. The authors also would like to thank Welspun Corp for the permission to publish this work.
Author information
Authors and Affiliations
Corresponding author
Rights and permissions
About this article
Cite this article
Goyal, R.K., Kyada, T. & Kathayat, T.S. Transverse Cracking of HF-ERW Pipes. J Fail. Anal. and Preven. 17, 370–375 (2017). https://doi.org/10.1007/s11668-017-0260-0
Received:
Revised:
Published:
Issue Date:
DOI: https://doi.org/10.1007/s11668-017-0260-0