Opening steel-pouring ladle slide gates without using oxygen1

  • REFRACTORIES IN HEAT UNITS
  • Published:
Refractories and Industrial Ceramics Aims and scope

In OAO Nizhnetagil Metallurgical Combine in order to open steel-pouring ladle slide gates without using oxygen starting mixes of domestic and imported production were checked instead of a quartzite starting mix.With their use the number of slide gate openings was 50%. Since this result should not be considered satisfactory, the search for suitable starting mixes continues.

This is a preview of subscription content, log in via an institution to check access.

Access this article

Price excludes VAT (USA)
Tax calculation will be finalised during checkout.

Instant access to the full article PDF.

Similar content being viewed by others

Author information

Authors and Affiliations

Authors

Additional information

Translated from Novye Ogneupory, No. 5, pp. 9 – 10, May 2010.

1From the proceedings of the International Conference of Metallurgists and Refractory Workers (April 22 – 23, 2010, Moscow).

Rights and permissions

Reprints and permissions

About this article

Cite this article

Visloguzova, É.A., Serova, L.V. & Khoroshikh, M.A. Opening steel-pouring ladle slide gates without using oxygen1 . Refract Ind Ceram 51, 135–136 (2010). https://doi.org/10.1007/s11148-010-9276-7

Download citation

  • Received:

  • Published:

  • Issue Date:

  • DOI: https://doi.org/10.1007/s11148-010-9276-7

Keywords

Navigation