Cork dust was consolidated without additives by heating under pressure. Four engineering properties of the compacted cork were measured: density, modulus, strength and fracture toughness. The thermal conductivity and the absorption of water by the compacted cork were also measured. The properties depend on the consolidation conditions, and (in a way which is not yet understood) on the origin of the cork dust itself, but not on particle size. The properties are compared with those of other common materials to identify possible uses.

This is a preview of subscription content, access via your institution.

References

  1. 1.

    J. V. Natividade, “Subericultura” (National Agronomics Institute. Ministry of Economics, Forestry Service, Lisbon, 1950).

    Google Scholar 

  2. 2.

    L. J. Gibson, K. E. Easterling and M. F. Ashby, Proc. R. Soc. Lond. A377 (1981) 99.

    Article  Google Scholar 

  3. 3.

    M. E. Rosa and M. A. Fortes, J. Mater. Sci. Lett. 7 (1988) 1064.

    CAS  Article  Google Scholar 

  4. 4.

    H. Pereira, M. E. Rosa and M. A. Fortes, Int. Ass. Wood Anatomists Bull. 8 (1987) 213.

    Google Scholar 

  5. 5.

    P. T. Lewis, Science 68 (1928) 635.

    Article  Google Scholar 

  6. 6.

    L. J. Gibson and M. F. Ashby, “Cellular Solids” (Pergamon Press, Oxford, 1987).

    Google Scholar 

  7. 7.

    A. Guillemonat, Ann. Fac. Sci. Marseille 30 (1960) 43.

    CAS  Google Scholar 

Download references

Author information

Affiliations

Authors

Rights and permissions

Reprints and Permissions

About this article

Cite this article

Flores, M., Rosa, M.E., Barlow, C.Y. et al. Properties and uses of consolidated cork dust. J Mater Sci 27, 5629–5634 (1992). https://doi.org/10.1007/BF00541634

Download citation

Keywords

  • Polymer
  • Particle Size
  • Dust
  • Thermal Conductivity
  • Fracture Toughness