The original version of this paper contained an error.

The first sentence in the “Materials and preparation” subsection under “Experimental” section should be changed.

From:

“In this study, a high-viscosity, natural PA 11 extrusion grade Rilsan BESNO TL from Atofina with a melting volume index of 1 cm3 (10 min) − 1 (235 °C, 2.16 kp) was used [1].”

To:

“In this study, high-viscosity extrusion-grade PA 11 Rilsan from Atofina was used [1]. It contained BBSA plasticizer, with its amount of less than 7.5 % controlled by blending neat (BESNO TL) and plasticizer-containing (BESNO P20 TL) grades.”